paul g wrote:Try scotchbrite with wd40 or brillo pads, rub backwards and forwards rather than randomly and it will give you a nice even grained satin look just like it came from the factory.
Leave the autosolve for the harley and Triumph boys!
you have got to rub with the grain of the metal if you go all over with it you will not get the heat in it to put a finish on it you just end up with a sore arm